Fractographic analysis of fractured lava ultimate crowns over zirconia abutments

Lohbauer, U., Schepke, U., Wendler, M. & Belli, R., 2016, In : DENTAL MATERIALS. 32, S1, p. e67

Research output: Contribution to journalMeeting AbstractAcademic